RENOLIN CKC |
|
100 |
150 |
220 |
320 |
460 |
680 |
|
Lubricating oil type |
|
|
|
|
|
|
|
|
acc. to ISO 6743-6 |
|
CKC 100 |
CKC 150 |
CKC 220 |
CKC 320 |
CKC 460 |
CKC 680 |
|
acc. to DIN 51 502 |
|
CLP 100 |
CLP 150 |
CLP 220 |
CLP 320 |
CLP 460 |
CLP 680 |
|
Characteristics |
Unit |
|
|
|
|
|
|
Test method |
Colour |
|
2 |
3 |
4 |
4.5 |
5 |
5 |
ASTM D 1500 |
Kinematic viscosity |
|
|
|
|
|
|
|
|
at 40 °C |
mm²/s |
94.4 |
145.6 |
214 |
331 |
468 |
690 |
ASTM D 445 |
at 100 °C |
mm²/s |
11.1 |
14.5 |
18.5 |
24.6 |
30.8 |
36.8 |
ASTM D 445 |
Viscosity index |
|
102 |
98 |
96 |
96 |
95 |
87 |
ASTM D 2270 |
Density at 15 °C |
kg/l |
0.884 |
0.89 |
0.895 |
0.9 |
0.903 |
0.922 |
ASTM D 1298 |
Flash point, Cleveland open cup |
°C |
220 |
225 |
230 |
230 |
240 |
245 |
ASTM D 92 |
Pour point |
°C |
– 27 |
- 24 |
- 21 |
- 15 |
– 12 |
– 12 |
ASTM D 97 |
Neutralization number |
mg KOH/g |
0.33 |
0.33 |
0.33 |
0.33 |
0.33 |
0.33 |
ASTM D 974 |
Saponification number |
mg KOH/g |
1.3 |
0.84 |
0.84 |
0.84 |
0.84 |
0.84 |
ASTM D 94 |
Sulphate ash |
% mass |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
0.1 |
ASTM D 874 |
Water content |
% mass |
not traceable |
not traceable |
not traceable |
not traceable |
not traceable |
not traceable |
ASTM D 95 |
Insolubles |
% mass |
not traceable |
not traceable |
not traceable |
not traceable |
not traceable |
not traceable |
DIN 51 592 |
Demulsification |
min |
< 20 |
< 20 |
< 20 |
< 20 |
< 20 |
< 20 |
DIN 51 599 |
Foaming, |
|
|
|
|
|
|
|
|
seq. I |
ml |
< 10/0 |
< 10/0 |
< 10/0 |
< 10/0 |
< 10/0 |
< 10/0 |
ASTM D 892 seq. I-III |
seq. II |
ml |
< 10/0 |
< 10/0 |
< 10/0 |
< 10/0 |
< 10/0 |
< 10/0 |
ASTM D 892 seq. I-III |
seq. III |
ml |
< 10/0 |
< 10/0 |
< 10/0 |
< 10/0 |
< 10/0 |
< 10/0 |
ASTM D 892 seq. I-III |
Copper corrosion |
degree of corr. |
1a-100A3 |
1a-100A3 |
1a-100A3 |
1a-100A3 |
1a-100A3 |
1a-100A3 |
ASTM D 130 |
Rust prevention |
|
pass B |
pass B |
pass B |
pass B |
pass B |
pass B |
ASTM D 665 |
Ageing behavior, |
|
|
|
|
|
|
|
|
viscosity increase |
% |
1 |
1 |
1 |
1 |
1 |
1 |
ASTM D 2893 |
precipitation number increase |
ml |
< 0.05 |
< 0.05 |
< 0.05 |
< 0.05 |
< 0.05 |
< 0.05 |
ASTM D 2893 |
FZG mechanical gear rig test |
load stage |
12 |
12 |
12 |
12 |
12 |
12 |
DIN 51 354-2 |
Effect on SRE-NBR 1 seal material acc to DIN 53 538-1 at 100 °C +/– 1 °C after 7 days +/– 2 hours, |
|
|
|
|
|
|
|
|
relative volume change |
% |
7 |
7 |
7 |
7 |
7 |
7 |
DIN 53 521 together with DIN 53 505 |
change in Shore A hardness |
Shore |
- 3 |
- 3 |
- 3 |
- 3 |
- 3 |
- 3 |
DIN 53 521 together with DIN 53 505 |